1. Study On The Mechanical Properties Of Laser Rapid Forming Of Rene'88DT Superalloy
2. Research On Purification Technology For The Master Alloy Of FGH96 Powder Superalloy
3. Study On Small Crack Propagation Behavior And Life Prediction Of FGH96 Powder Superalloy
4. Simulation Of Broaching Of FGH95 Nickel-base Superalloy And Optimization Of Broach Parameters
5. Study On Microstructure And Mechanical Properties Of Powder Superalloy FGH96/97
6. Identification Of FGH97 Superalloy Material Characteristic Parameters And Optimization Of Machining Parameters
7. Research On The Evaluation Of Fatigue Microcrack Expansion Of Powder Superalloy Based On Ultrasound
8. Research On Hot Deformation Behavior Of FGH4096 Nickel-based Powder Superalloy