21.
Study On Small Hole Drilling Technology Of Superalloy
22.
Study Of The Dynamic Compression Mechanical Behavior Of Laser Solid Formed GH4169 Superalloy
23.
Microstructure And Mechanical Properties Of Laser Repaired GH4169 Superalloy Assisted By Electromagnetic Stirring
24.
Microstructure And Mechanical Properties Of Nb Modified GH4169 Superalloy Produced By Laser Additive Manufacturing
25.
Processing Characteristics,Macro/microstructure And Mechanical Properties Of GH4169 By CMT Arc Additive Manufacturing
26.
Research On Fatigue And Wear Properties Of GH4169 Alloy With Gradient Nanostructure
27.
Three Dimentional EBSD-based Microstructure Reconstruction And Micro-mechanical For GH4169 Superalloy
28.
Experimental And Modelling Study On The Residual Stress In GH4169 Superalloy
29.
GH4169 Superalloy Multi-directional Forging Process And Simulation Study Of Microstructure Evolution
30.
Microstructure And Properties Of Zr-ti Alloy By Liquid Phase Spark Sintering Of Zr-Ti Alloy Powder Using GH4169 Powder As Auxiliary Agent
31.
Effect Of The Initial Microstructure Of GH4169 Superalloy On Microstructure And Properties Of Welded Joint
32.
Study On Macroscopic And Microscopic Laws Of GH4169 Superalloy Shafts In Cross Wedge Rolling
33.
Effect Of Milling Parameters On Surface Integrity And Low Cycle Fatigue Performance Of GH4169 Superalloy
34.
Experimental And Modeling Investigations Of The Heat-treatment Residual Stress Evolution In GH4169 Superalloy
35.
Research On Temperature Field Stress Field Of GH4169 Superalloy Made By Laser Additive Manufacturing
36.
Research On Optimization Of Oblique Laser Shock Processing Parameters Of GH4169 Superalloy
37.
Investigation On Formation Mechanism Of Deteriorative Layer On Machined Surface Of GH4169 Superalloy Under High-Pressure Cooling
38.
Study On Friction And Cooling Characteristics Of Nanofluid Minimum Quantity Lubrication Milling GH4169 Superalloy
39.
Methods For Predicting Creep Life Of GH4169 Superalloy
40.
Powder Recycling Of GH4169 Superalloy Laser Cladding Homogenous Repairing